4.Control the content of Mn and the coiling temperature of hot rolling to optimize the material.
In order to improve the deep drawing formability of steel sheet, it is necessary to reduce its influence to a minimum when processing with cementite in the presence of cementite except for no solid solution carbon. Therefore, the composition of the steel is adjusted and the rolling temperature is controlled.
In the past, hot rolled steel sheets were coiled at high temperature before cold rolling. Because the cooling after coiling is very slow, the cementite formed is coarse, can reduce the place where turbulence occurs during the processing, and most of the carbon is aggregated into the cementite during the slow cooling process. However, the higher the coiling temperature of hot rolled strip, the greater the difference of cooling rate between surface and interior, which makes the dispersion degree of cementite and the amount of carbon dissolved in solid solution fluctuate, and even makes the crystal direction of some iron atoms not fully consistent. In order to avoid this situation, it is most effective to reduce the coiling temperature of hot rolling. In addition, the growth rate of cementite is analyzed in detail. The results show that when the content of Mn in steel is reduced, the cementite is easy to be coarse even when it is coiled at low temperature. Therefore, the ideal shape of carbon and cementite can be controlled even if the hot rolled sheet is coiled at relatively low temperature, so as to stabilize the deep drawing formability of the steel plate.
5.The ideal crystal orientation of IF steel can be obtained by means of composition adjustment, temperature management and controlled rolling.
Due to the complexity of the car body shape and the integration of the separated parts, the outer plate of the car must have harsh deep drawing formability. Therefore, the lower carbon (0.01% / 0.05%) steel must be further reduced in the steelmaking process, and the lower carbon (0.01% / 0.05%) steel must be further reduced in the steelmaking process. To achieve ultra-low carbonization (pure iron).
The key of pure iron process is to reduce carbon and impurities to the limit. By means of vacuum degassing secondary refining process, the molten steel at the end of converter blowing is further degassed in the vacuum tank (including decarbonization, denitrogenation and decarbonization), and the carbon content in the molten steel is reduced to less than 10ppm (i.e. 0.001%).
If a proper amount of micro-alloying elements such as Ti and Nb are added to the molten steel which is similar to pure iron, there is only harmless carbon in the steel, which is called IF steel. If the recrystallization process of the hardened grains from cold rolling is observed during annealing, it is found that the grains produced by the boundary (i.e. grain boundary) between the grains before cold rolling have a tetrahedral crystal orientation with a high r value which can promote the improvement of the deep drawing property. In order to provide as many crystal boundaries as possible, the grain size should be controlled as much as possible before cold rolling. Therefore, the heating temperature should be lowered at the beginning of hot rolling, and hot rolled at low temperature as far as possible, so that the steel can be cooled before the grain size is large.
In addition, the addition of Ti and Nb is adjusted to the optimum conditions for grain refinement. The difference between if steel and low carbon steel is that the carbon in steel is fixed by microalloying elements Ti and Nb, so there is no need to worry about aging deterioration caused by residual carbon. At present, many Japanese steelmakers, represented by Nippon Railway, adopt steelmaking, rolling technology and high precision temperature control technology from hot rolling to continuous annealing to continuously produce high quality IF steel which meets the requirements of harsh deep drawing.
6 .soft and rugged BH steel plate
The outer plate of the automobile shall be soft and beautiful Mn content view, and after the car is finished, it must also have the characteristics of resistance to impact, for example, no depression will occur in the event of a small stone impact or a collision between the car park and the car door of the adjacent car. In order to make the sheet of < 1mm thickness have this characteristic, the steel plate must be hard, but the hard steel sheet is difficult to form, and the local wrinkle caused by stamping is also harmful to the appearance.
Therefore, BH steel plate was developed. It is characterized by soft forming but hardening when the finished product is used. This is due to the extremely small amount of solid solution carbon remaining in the steel plate, which migrates in the steel during the drying process of the painted car body (170 ℃ × 20min), thus inhibiting the slip deformation of the steel (even if the steel plate becomes hardened). The addition of Ti and Nb is controlled and optimized by Nippon Iron, and the performance of the product is stable after 6 months storage at room temperature. The developed BH steel plate has been applied and is contributing to the thin-walled and light-weight of vehicle outer plate.
If you want to know more about iron sheet metal punch service and sheet metal products with powder costing. please email below.