Shenzhen prototype factory will use die casting when making prototype. Die casting is a kind of metal casting process, which is characterized by applying high pressure to molten metal by using mold cavity, which is similar to plastic injection molding. Die-casting is especially suitable for the manufacture of a large number of small and medium-sized castings, so die-casting is one of the most widely used in various casting processes. Compared with other casting technologies, die casting has a smoother surface and higher size consistency. However, non-standard operation and parameters can also produce a variety of defects.

I, streaks and patterns.
Appearance check:
There are stripes on the surface of the casting which are consistent with the flow direction of the liquid metal, and there are obvious non-directional patterns with different colors from the metal matrix, and there is no trend of development.
The flow marks are caused by the following:
(1) the mold temperature is too low;
(2) the gate design is not good;
(3) the material temperature is too low;
(4) the filling speed is low and the filling time is short;
(5) the gating system is unreasonable;
(6) exhaust gas is bad;
(7) spray is unreasonable.
II. Tortoise crack
Appearance check:
The surface of die casting has the marks of reticulated hair protruding or sagging, which expands and extends with the increase of die casting times.
The reasons are as follows:
(1) there are cracks on the surface of die-casting die cavity,
(2) the preheating of die-casting die is not uniform.
III. cold partition
Appearance check:
The surface of die castings has obvious, irregular and linear patterns (with and without penetration). The shape of die casting is small and narrow, sometimes the interface edge is smooth, and it is possible to break under the action of external force.
The reasons are as follows:
(1)The two strands of metal are interfaced with each other, but they are not completely fused and there is no inclusion in the two strands, and the bonding force of the two strands is very weak.
(2) the pouring temperature or die casting die temperature is lower;
(3) the runner position is not right or the flow path is too long;
(4) the filling speed is low.
IV, indentation
Appearance check:
There are smooth indentation (like a disc) on most of the thick surface of a die casting. There are smooth indentation (like a disc) on most of the thick surface of a die casting.
The reasons are as follows:
(1) caused by contraction
The wall thickness difference of die casting is too big;
Improper location of the sprue;
The pressure-ejection ratio is low and the holding time is short.
The local temperature of die casting die is too high.
(2) the design of cooling system is unreasonable;
(3) the mould opening is premature;
(4) the pouring temperature is too high.
Delamination (covering and stripping)
Appearance check or damage check:
There is a distinct layer of metal in the part of the casting.
The reasons are as follows:
(1)Die rigidity is not enough in the process of liquid metal filling, the template jitter;
(2)In the process of pressing the punch appeared crawling phenomenon;
(3) improper design of runner system.

If you want to know more about resin 3d printing rapid prototype and pc material sla 3d printing service. please email below.